Loading efficiency of siRNA in PK3 or PLGA particles and particle sizes

Submicron particles PK3–siRNA particle without chloroquine PK3–siRNA particle with chloroquine (PKCN–siRNA) PLGA–siRNA particle with chloroquine
Average loading efficiency (%)a 42.43 59.05 47.95
Particle size (nm)b 934.2 ± 59.3 887.7 ± 56.7 881.0 ± 514.9

aThe loading efficiency of Fl-siRNA in the PKCNs was determined by fluorescence of fluorescein (λexem = 494/518 nm). Loading efficiency (%) = (amount of Fl-siRNA loaded in submicron particle)/(initial amount of Fl-siRNA used to make submicron particle) × 100.

bParticle size was determined by DLS (mean ± SD).